High Temperature Rupture Creep Testing Machine

application

         The tester is used to test the mental and non-mental,such as tension, compression
rupture,relaxation test,high temperature tensile,etc.The test meet GB、HB and other
relevant standards.

detailed information

15  

Satisfying and applicable standard

 

 

GB/T 2039-2012              Metallic materials—Uniaxial creep testing method in tension
HB 5150                            Metallic materials―Rupture testing at elevated temperature
HB 5151                            Metallic materials―Creep testing at elevated temperature
ASTM E139                      Standard Test Method for Conducting Creep,Creep-Rupture,and 
                                           Stress-Rupture Tests of Metallic Materials
ASTM E292                      Standard Test Methods for Conducting Time-for-Rupture 
                                           Notch Tension Tests of Materials
JJG 276-2009                 Verification Regulation of High-Temperature Creep and 
                                           Stress-Rupture Testing Machines
JJG 351                            Verification Regulation of Working Base Metal Thermocouple

 

 

 

Performance parameter

Model

RMT-D3

RMT-D5

RMT-D10

Testing force range(kN)

30kN

50kN

100kN

Accuracy grade

0.5 Class

Testing force range

0.4%--100% FS 

Testing force accuracy

<0.5

Testing force resolution

1/350000 of maximal force

Designed by three 

section temperature controled

Temperature range

200~1100

Temperature precision

Satisfied HB5195-96B

Uniform temperature zone length

150mm

High temperature 

furnace specifications

Inside diameter, outside diameter,length configured according to the standard,

aslo to the user requirements.

Temperature control method

Direct type (Thermocouple tied the sample)  indirect type(Thermocouple accessed from the furnace side)

Temperature fluctuation

 600        ±2

 600~900    ±3

 >900         ±4

Temperature gradient

 600         2

 600~900     3

 >900          4